Step 2 - Print Setting
Model Setup
- Scale & Size – Too small → loss of detail; too large → longer print time
- Orientation – Poor angles can cause rough surfaces or weak layer bonding
- Supports – Missing or excessive supports can lead to surface marks or print failure
- Support Overhang Angle: 45°
Layer Settings
- Layer Height (recommended: 0.12 – 0.3 mm) – Smaller height → smoother surface, longer print time
- Wall Line Count (recommended: 2 – 8) – More walls → stronger print, longer print time
- Infill Density (recommended: 5% – 30%) – Lower infill → faster print, but weaker structure
Temperature & Speed
- Nozzle Temperature (Recommended temperature for PLA: 215. Temperature varies by filament type) – Too low → poor adhesion and print failure; too high → stringing, blobs, or print failure
BedBuild Plate Temperature (set to 75 °C) – Too low → warping and print failure; too high → overly sticky bottom layers
- Print Speed – Higher speed generally results in lower print quality
Adhesion & Environment
- Bed Adhesion Type (recommended: Brim) – Skirt / Brim / Raft affects print stability
- Levelling – Uneven or dirty print beds cause poor first-layer adhesion
- Ambient Conditions – Drafts or vibrations can distort printed layers